"H": Catching and holding the peak value in test.
"OFF/ON": Power off and Power on
"ZERO": Self-Calibration
Note:
Please let us know the model you need before buying.A,C,D
1.Introduction:
SHORE-A DUROMETER :It is designed for testing the hardness of soft
rubber,printer roller and other elastomer material.(ASTM--D--2240)
SHORE-D DUROMETER:It is designed for testing the hardness of hard rubber,such
as:thermoplastic plastics,bowling,plastic floor and so on.(ASTM--D--2240)
SHORE-C DUROMETER:It is designed for the hardness of soft and elasticty
material,spinning trunk rotation and soft grain structure
materials.(ASTM--D--2240)
2.Parameters:
| Model | Force | Pressure | Shape of measuring head | Length of Probe | Dial Scale |
| A | 8.1N | 1Kg | Top angle(35angle) | 2.5mm | 0-100mm |
| D | 44.5N | 5Kg | Top angle(30angle) | 2.5mm | 0-100mm |
| C | 8.1N | 1Kg | Spheric radius2.38mm | 2.5mm | 0-100mm |
3.Notice:
1).Thickness of test specimen >6mm,no more than 3 layers; Test area >/=feet
area(diameter 18mm).
2).Test 3 times and calculate the average as test result.
3).Usually,plz use A/D.When the hardness of A >90,plz use D or C.