High Temp Brushed Bronze

Low Cure Specialty Silicone Based Powder Coating for High Temperature Applications (600F – 1200F)

Cure Schedule = 400F/15 min at Part Metal Temperature

Gloss Level = 10-20% on 60 Degree Meter Scale

Recommended Mil Thickness = 1.0-1.5 Mils.

Specific Gravity = 2.00

Theoretical Coverage = 45.0 Sq. Ft.

Salt Spray Results = 1,000+ Hours

* ZINC OR IRON PHOSPHATE CANNOT BE USED ON SUBSTRATE BEFORE APPLYING HIGH TEMP POWDERS

* THIS PRODUCT CANNOT BE SECOND-COATED

Due To The Temperature Sensitive Nature Of High Temp Powders From May 1 – September 30, Expedited Shipping Is Required And Should Not be Shipped Over The Weekend. We Are Not Responsible For Heat Damage and Product Loss