2.Printing fluidity is 500% higher than PLA, printing at speeds above 250mm/s without clogging.
3.Thermal performance is 180% better than PLA and models cool faster under the same printing conditions.
4.Fast printing at 180~195℃ low temperature, saving time and energy consumption.
5.Strong toughness low shrinkage, printing without cracking, smooth surface of the model.